Vermiculite Spiral Wound Gasket: Specs, Applications and Thermiculite 835 Comparison

When a graphite-filled spiral wound gasket keeps failing on a hot line, the filler is usually the problem, not the metal. Flexible graphite oxidizes in air at high temperature, loses weight, and the joint starts to leak after a few thermal cycles. A vermiculite spiral wound gasket solves this by replacing graphite with an inorganic mineral filler that does not oxidize. This guide explains how the vermiculite filler works and gives the technical data for our FS-G002 vermiculite spiral wound gasket. It covers where to use it, how to specify it, and how it compares with Flexitallic Thermiculite® 835.
What Is a Vermiculite Spiral Wound Gasket?

A spiral wound gasket is made by winding a V-shaped metal strip and a soft filler tape together in a spiral. The metal gives strength and recovery; the filler does the sealing. In a vermiculite spiral wound gasket, the filler is a tape made from chemically exfoliated vermiculite.
Vermiculite is a natural layered silicate mineral. Through chemical and thermal exfoliation it is split into very thin platelets and then calendered into a soft, compressible tape, much like expanded graphite. The difference is that vermiculite is a mineral: it does not burn and does not oxidize in air. That single property is why refineries and chemical plants move to vermiculite filler on fired heaters, reformers and other hot, oxidizing joints.
Why Choose Vermiculite Filler Instead of Graphite?
Flexible graphite is still the best general-purpose filler. It is easy to seal and low in cost. Its weak point is oxidation:
- In air, flexible graphite begins to oxidize at roughly 450 °C. For multi-year service the safe limit is lower still. Long-term test data published by gasket manufacturers put it in the 300–370 °C range, depending on service life.
- Oxidation causes weight loss of the filler. That leads to loss of gasket stress, leakage and, on heaters and furnaces, repeated gasket replacement.
- Strong oxidizers such as concentrated nitric acid attack graphite even at lower temperatures.
Vermiculite filler removes this limit. It stays stable in hot air and oxidizing media and under severe thermal cycling, up to about 1,000 °C for the filler itself.
| Item | Vermiculite filler | Flexible graphite filler |
|---|---|---|
| Oxidation in air | Does not oxidize | Oxidizes above about 450 °C |
| Filler temperature limit (typical) | About 1,000 °C | About 450 °C in air; about 650 °C in steam / non-oxidizing service |
| Fire behavior | Non-combustible mineral | Good, but oxidation is the weak point |
| Strong oxidizing media | Suitable | Not recommended |
| Conformability at low bolt load | Good, slightly below graphite | Excellent |
| Cost | Higher | Lower |
Rule of thumb: below about 450 °C in air, a graphite-filled gasket is usually the economical choice. Above that, or wherever graphite gaskets keep failing from oxidation, specify vermiculite filler.
FS-G002 Vermiculite Spiral Wound Gasket: Technical Specifications

Our FS-G002 Spiral Wound Gasket is available with vermiculite filler in all standard styles:
- R: sealing element only, for tongue-and-groove or male-and-female flanges
- CG: with outer centering ring
- CGI: with outer centering ring and inner ring (recommended for most raised-face flanges and high-temperature service)
- RIR: with inner ring only
| Parameter | FS-G002 (vermiculite filler) |
|---|---|
| Filler | High-temperature chemically exfoliated vermiculite tape |
| Winding metal | SS304, SS316 / 316L, SS321, Inconel 600 / 800, Hastelloy B2, titanium, duplex |
| Inner / outer ring | Carbon steel, SS304, SS316L or to match the winding |
| Filler temperature limit | Up to 1,000 °C* |
| Max. pressure | 250 bar (450 bar with special winding strip) |
| Filler density | 1.1 – 1.3 g/cm³ |
| Leachable chloride / fluoride | Each < 50 ppm |
| Recovery | Up to about 30% |
| Thickness | 3.2 / 4.5 / 6.4 mm; others on request |
| Standards | ASME B16.20 (B16.5 and B16.47 Series A / B flanges), EN 1514-2, JIS B2404, or to drawing |
| Documents | Test report from the vermiculite raw material supplier; fire testing can be arranged per project on request |
*Typical values. The service limit of a finished gasket is the lower of the filler and winding metal limits. For example, SS316L winding is typically rated to about 760 °C. Above that, choose an Inconel winding. Final data are per batch test reports.
ASME B16.20 Notes for Vermiculite Gaskets
- Abbreviation: ASME B16.20-2023 does not assign an abbreviation to vermiculite (graphite is FG, PTFE is PTFE). The filler marking on the ring is agreed with the buyer.
- Inner ring: regardless of filler, ASME B16.20 requires an inner ring for Class 900 NPS 24 and larger, Class 1500 NPS 12 and larger, and Class 2500 NPS 4 and larger. For high-temperature service we recommend the CGI style in general.
Typical Applications
Vermiculite spiral wound gaskets are used where temperature, oxidation or thermal cycling defeats graphite:
- Refining and petrochemicals: fired heater outlets, reformers and re-reformers, FCC units, ethylene cracking heaters, dehydrogenation units, hot hydrocarbon lines
- Chemicals and fertilizer: ammonia plants, nitric acid and other strong oxidizers, methanol-to-olefins (MTO) units
- Power generation: superheated steam, boiler saturated steam, gas turbine exhaust, heat recovery steam generators (HRSG)
- New energy: molten salt systems in solar thermal plants, waste-to-energy, biofuel plants
- Any joint where graphite gaskets have shown weight loss, oxidation or repeated leakage after thermal cycles
FS-G002 (Vermiculite Filler) vs. Thermiculite® 835

Many inquiries name Flexitallic Thermiculite® 835, the best-known vermiculite spiral wound filler. FS-G002 with vermiculite filler is an equivalent product for the same type of service. Here is how the published figures compare:
| Item | FS-G002 (vermiculite filler) | Flexitallic Thermiculite® 835 |
|---|---|---|
| Styles | R / CG / CGI / RIR | R / CG / CGI / RIR |
| Standards | ASME B16.20 / EN 1514-2 / JIS B2404 | ASME, DIN, EN and others |
| Filler | High-temperature vermiculite tape | Thermiculite 835 |
| Winding metal | SS304, SS316(L), SS321, Inconel 600/800, Hastelloy B2, titanium, duplex | Typically 316L, others available |
| Max. temperature (filler) | 1,000 °C | 980 °C |
| Max. pressure | 250 bar (450 bar with special strip) | ASME B16.5 Class 2500 |
| Filler density | 1.1 – 1.3 g/cm³ | 1.2 – 1.3 g/cm³ |
| Chloride / fluoride | Each < 50 ppm | Each < 50 ppm |
| Recovery | Up to about 30% | — |
| Thickness | 3.2 / 4.5 / 6.4 mm, others to order | 1.6 – 7.2 mm |
| Fire test | On request per project | API 6FB |
How to read this comparison:
- Temperature, density and chloride/fluoride figures are in the same range. Both fillers are designed for the same hot, oxidizing service.
- Thermiculite 835 carries an API 6FB fire-safe listing and a published Class 2500 rating. If your project specification requires a certified fire test or a named OEM, tell us at the inquiry stage. We will confirm what can be provided before quoting.
- FS-G002 offers a wider choice of winding metals and is supplied factory-direct, typically at a more competitive price for maintenance, turnaround and replacement orders.
Thermiculite® is a registered trademark of Flexitallic. Flexitallic data are quoted from its public datasheet for comparison only. FS-G002 is manufactured for Felix Sealing and is not a Flexitallic product.
How to Specify and Order
To get an accurate quotation quickly, please include:
- Style: R / CG / CGI / RIR
- Size: NPS + pressure class + flange standard (ASME B16.5, B16.47 Series A or Series B, EN, JIS), or a drawing
- Winding metal (e.g. SS316L, Inconel 600)
- Filler: vermiculite (state if it replaces Thermiculite 835)
- Inner and outer ring material
- Service conditions: temperature, pressure and medium
- Quantity and required documents
Need a ring joint gasket for the same line? See our FS-G003 Ring Joint Gasket.
FAQ
What temperature can a vermiculite spiral wound gasket handle?
The vermiculite filler is rated to about 1,000 °C. The finished gasket is limited by the winding metal. Typical limits are about 760 °C for SS316L and up to about 1,090 °C for Inconel 600 / 625.
Is vermiculite better than graphite?
Not in every case. Graphite seals more easily and costs less, and it is the right choice below about 450 °C in air. Vermiculite is better for hot, oxidizing or severe thermal-cycling service where graphite oxidizes.
Can FS-G002 replace Thermiculite 835?
FS-G002 with vermiculite filler is designed as an equivalent for the same service and shares the same styles and similar filler data. Where a project requires the OEM brand or an API 6FB certificate, please tell us before quoting.
Is the vermiculite asbestos-free?
Sealing-grade vermiculite is processed to be asbestos-free, and we supply the vermiculite raw material supplier’s test report with the order. If your project requires a specific asbestos test report, please tell us at the inquiry stage.
Get a Quote for Vermiculite Spiral Wound Gaskets
Send us your sizes, materials and service conditions. We usually reply within 12 hours with a quotation and lead time. Samples can be arranged. Full specifications: FS-G002 Spiral Wound Gasket.